EFFECT OF PVD TI DEPOSITION TIME ON THE CORROSION BEHAVIOR OF AISI 431 MARTENSITIC STAINLESS STEEL


Tamer F. B., Çanakçı A., Tunç S. A.

16th International Azerbaijan Congress on Life, Engineering, Mathematical, and Applied Sciences, Baku, Azerbaycan, 20 - 22 Eylül 2026, ss.203-210, (Tam Metin Bildiri)

  • Yayın Türü: Bildiri / Tam Metin Bildiri
  • Basıldığı Şehir: Baku
  • Basıldığı Ülke: Azerbaycan
  • Sayfa Sayıları: ss.203-210
  • Karadeniz Teknik Üniversitesi Adresli: Evet

Özet

AISI 431 martensitic stainless steel possesses a favorable combination of mechanical strength, hardness, and wear resistance; however, its electrochemical stability may become limited under chloride-rich service conditions. In this study, the corrosion behavior of Ti-coated AISI 431 stainless steel was systematically investigated as a function of physical vapor deposition (PVD) duration. Titanium coatings were deposited by RF magnetron sputtering for 30, 60, and 90 min, and the corresponding specimens were designated Ti-30, Ti-60, and Ti-90, respectively. Deposition duration was selected as the primary variable, while the remaining coating parameters were maintained constant. The electrochemical performance of the coated specimens was evaluated by potentiodynamic polarization testing in 3.5 wt.% NaCl solution, and the resulting Tafel curves were comparatively analyzed in terms of corrosion potential and current-density response. The polarization behavior revealed pronounced differences among the three coating conditions. Ti-30 exhibited the most positive corrosion-potential region, located at approximately  0.18 V, indicating a comparatively noble electrochemical potential. Nevertheless, its polarization curve was shifted toward substantially higher current densities, demonstrating that a more positive corrosion potential alone did not correspond to the lowest corrosion  inetics. In contrast, Ti-60 and Ti-90 exhibited markedly lower current-density responses in the vicinity of their respective corrosion potentials. Ti-90 showed the lowest characteristic current-density region, with Ti-60 displaying a slightly higher but still comparatively low current response.  Accordingly, the corrosion resistance based on the overall Tafel response decreased in the following order: Ti-90, Ti-60, Ti-30. The results demonstrate that the electrochemical performance of PVD-deposited Ti coatings cannot be assessed exclusively from the positive  isplacement of corrosion potential. Rather, the magnitude of the corrosion current density provides a more direct indication of the kinetics of metallic dissolution under chloride exposure. Although Ti-30 exhibited the noblest potential, its comparatively high currentdensity response  ndicated greater electrochemical activity. Conversely, reduced current-density levels of Ti-90 and Ti-60 reflected more effective suppression of corrosion reactions. Among the investigated coating durations, the 90 min Ti deposition condition provided the most favorable overall  corrosion response in 3.5 wt.% NaCl solution.