The effect of heat treatment on microstructural, mechanical and tribological properties of Ti-Ag alloy produced by selective laser melting method


Creative Commons License

AKÇAY S. B., VAROL T., GÜLER O., ÇUVALCI O., AKSA H. C., BEDER M., ...Daha Fazla

Scientific Reports, cilt.16, sa.1, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 16 Sayı: 1
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1038/s41598-026-65506-4
  • Dergi Adı: Scientific Reports
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, BIOSIS, Chemical Abstracts Core, EMBASE, MEDLINE, Directory of Open Access Journals, Zoological Record, Academic Search Ultimate (EBSCO), Natural Science Collection (ProQuest), Biological Science Database (ProQuest), Biomedical Reference Collection: Corporate Edition (EBSCO), Health Research Premium Collection (ProQuest)
  • Anahtar Kelimeler: Additive Manufacturing, Friction, Heat treatment, Selective Laser Melting (SLM), Ti–Ag alloy, Wear
  • Açık Arşiv Koleksiyonu: AVESİS Açık Erişim Koleksiyonu
  • Karadeniz Teknik Üniversitesi Adresli: Evet

Özet

This study systematically investigated the effects of different post-fabrication heat treatments on the microstructural, mechanical, and tribological properties of a novel Ti-Ag alloy produced by selective laser melting (SLM). Unlike conventional powder mixing methods reported in the literature, electroless Ag-coated Ti powders were used as feedstock, enabling controlled Ag distribution in the Ti matrix through post-SLM heat treatments. X-ray diffraction analysis confirmed that the α-Ti-based matrix structure was preserved in all samples, while oxide phases formed after heat treatment. The water-cooled and aged specimen (HT-3) exhibited the highest hardness (508.9 ± 13 HV), corresponding to a 68.8% increase compared to the untreated SLM specimen. This improvement was attributed to Ag-rich precipitate formation and stabilization of rutile/anatase phases. Tensile testing showed that the as-built SLM specimen had the highest tensile strength (639.5 MPa), whereas heat-treated samples showed reduced strength due to oxidation and microstructural changes during cooling. Under 15 N load and 100 m sliding distance, heat-treated specimens demonstrated significantly lower friction coefficients, with HT-3 reaching 0.48 (22.6% reduction). HT-3 also exhibited the lowest volume loss, indicating superior wear resistance and stable friction behavior.